Dapping Recipe & Parameters
模具压窝(Dapping)配方与参数
标签:压窝, 半圆冲, 凹模, 槌击, 参数
选与凹模孔径匹配的金属半圆冲(dapping punch),将退火圆片放入对应凹坑,冲头对准中心,用木槌或软面槌垂直敲击冲尾数次,使片材贴合模腔成半球。紫铜片厚 0.5–1.0 mm 为宜;过厚难成形,过薄易起皱。每打几槌检查贴合度。
Pick a dapping punch matching the block bore, seat the annealed disc in the matching cavity, centre the punch and strike its tail vertically a few times with a mallet so the sheet conforms to the hemisphere. Copper 0.5–1.0 mm works best; too thick won't form, too thin wrinkles. Check fit every few blows. ---